Hello Guys

Can anyone recomend a spray tack for epoxy resin infusion ?

I Infused a part on the weekend using Infuzene and it left stringy marks on the surface. Maybe i used to much but it sprays so inconsistently , hard to get only a mist.

I live in Australia so any local help with suppliers would be great.

Thanks

Rod.
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Oh well there you go! 

It does work well for infusion, I use it for everything. It has a mix viscosity of 300-400cps at 25 degrees, so it is a touch slower than the 200cps R118. This only really becomes an issue if you are doing a large part using an internal flow media like Soric, and you don't want to help flow with external mesh. But I have infused a 2.7sqm bonnet using only Soric, and that infused fully in about 40 minutes, so still no where near your pot life. If it does become an issue, just mix smaller batches and refill the pot a few times.

I highly recommend giving it a go instead of the kinetix. 
Edited 10 Years Ago by Hanaldo
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
rallyfly - 10 Years Ago
Hanaldo - 10 Years Ago
rallyfly - 10 Years Ago
Hanaldo - 10 Years Ago
rallyfly - 10 Years Ago
MarkMK - 10 Years Ago
rallyfly - 10 Years Ago
Hanaldo - 10 Years Ago
rallyfly - 10 Years Ago
Hanaldo - 10 Years Ago
rallyfly - 10 Years Ago
ChrisR - 10 Years Ago
rallyfly - 10 Years Ago
Warren (Staff) - 10 Years Ago
Chris Scott - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search