Depending on how much your going to do you might like to try
Wurth Sabasto Replast easy
Its used to repair plastic bumpers so sticks without all the other hassle
Also unlike 99% of other glues when it sets it doesn't go hard and brittle it still has a bit of flex
Also sticks to carbon Very well
comes in 3 different speeds an is designed to be used with a applicator gun and mixer nozzles which can work out expensive but most of the time we forget about the nozzles and just use the gun to dispence onto a mixing board an mix by hand
|