Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Use carbon fiber part to fix/reinforce ABS parts
Use carbon fiber part to fix/reinforce ABS parts
Post Reply
Like
4
Use carbon fiber part to fix/reinforce ABS parts
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
ducatichiang
ducatichiang
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 29
Hi everyone,
Sorry for my poor English.
I want to use carbon fiber to fix/reinforce my scooter ABS parts.
The plan is make some carbon fiber tenon(Sorry. I am not sure how to call it in English...) to replace original
tenon on the
part.
Please refer to the red mark in the picture.
I need make two materials stick together(ABS and carbon fiber).
The question is what kind of adhesive should I use?
E515, ET500, ET538, PT326, PU18 or others solution/advised?
Best Regards & Thanks
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Use carbon fiber part to fix/reinforce ABS parts
ducatichiang
-
10 Years Ago
The ABS needs to be treated to allow the epoxy to bond. CLEAN ABRADE (400grit) CLEAN FLAME TREAT...
ChrisR
-
10 Years Ago
Chris is correct with the preparation and epoxy will bond when used in this way. However we would...
Warren (Staff)
-
10 Years Ago
Depending on how much your going to do you might like to try Wurth Sabasto Replast easy Its used...
f1rob
-
10 Years Ago
Thank you all of you!! These information are very useful and important to me. Best Regards &...
ducatichiang
-
10 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search