Is clear polyester resin suitable for encapsulating a rough bit of yew wood with bark on?


Is clear polyester resin suitable for encapsulating a rough bit of yew wood with bark on?
Poll
Is clear polyester resin suitable for encapsulating a rough bit of yew wood with bark on? Closed

I have researched the resin thoroughly but need advice.
0% - 0 votes
Member Votes: 0, Guest Votes: 0. This poll has been closed and is not accepting new votes
Author
Message
jruck
jruck
Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)
Group: Forum Members
Posts: 2, Visits: 7
Hi I am new to resins and for a school project have got hold of a piece of yew wood. My plan is to encapsulate the sanded bit of yew within the clear resin. I am going to use the resin to fill out the edges of the wood so that it is square because the wood has a rough jagged edge with bark still on. The project is to be a coffee table. The rectangular size for the whole table will be 88x64x5cm so it is fairly large. I have calculated the amount of resin needed and will be roughly 5kg worth of it. I will make a plywood box for the mould lined with mould release. Is clear polyester resin suitable for this table and if so would I be able to do the resin in one go.
Many thanks 
Reply
jruck
jruck
Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)
Group: Forum Members
Posts: 2, Visits: 7
Many thanks,
However if I pour the resin in multiple layers would the layers be visible because i am trying to go for as transparent a finish as possible.
Would it make any difference if i was to use slightly less catalyst in order to keep heat down?

Thanks for your help!