Is clear polyester resin suitable for encapsulating a rough bit of yew wood with bark on?


Is clear polyester resin suitable for encapsulating a rough bit of yew wood with bark on?
Poll
Is clear polyester resin suitable for encapsulating a rough bit of yew wood with bark on? Closed

I have researched the resin thoroughly but need advice.
0% - 0 votes
Member Votes: 0, Guest Votes: 0. This poll has been closed and is not accepting new votes
Author
Message
jruck
jruck
Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)
Group: Forum Members
Posts: 2, Visits: 7
Hi I am new to resins and for a school project have got hold of a piece of yew wood. My plan is to encapsulate the sanded bit of yew within the clear resin. I am going to use the resin to fill out the edges of the wood so that it is square because the wood has a rough jagged edge with bark still on. The project is to be a coffee table. The rectangular size for the whole table will be 88x64x5cm so it is fairly large. I have calculated the amount of resin needed and will be roughly 5kg worth of it. I will make a plywood box for the mould lined with mould release. Is clear polyester resin suitable for this table and if so would I be able to do the resin in one go.
Many thanks 
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You would see a very slight transition from the side.  Reducing the catalyst ratio would help a little too but that also depends on the ambient temperature. If it is very cool 15C or below, you may find a low catalyst ratio means the resin takes a very long time to cure.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Warren great idea to dip the wood in the resin first, never thought of that before. 
But how about moist trapped in the wood and bond between the dipped (cured) wood and the extra resin coming on top?

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search