Is clear polyester resin suitable for encapsulating a rough bit of yew...
Is clear polyester resin suitable for encapsulating a rough bit of yew wood with bark on?
Post Reply
Like
13
Is clear polyester resin suitable for encapsulating a rough bit of yew wood with bark on?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Poll
Is clear polyester resin suitable for encapsulating a rough bit of yew wood with bark on?
Closed
I have researched the resin thoroughly but need advice.
Member Votes: 0, Guest Votes: 0.
This poll has been closed and is not accepting new votes
Author
Message
jruck
jruck
posted 11 Years Ago
ANSWER
HOT
Poll Details
Group: Forum Members
Posts: 2,
Visits: 7
Hi I am new to resins and for a school project have got hold of a piece of yew wood. My plan is to encapsulate the sanded bit of yew within the clear resin. I am going to use the resin to fill out the edges of the wood so that it is square because the wood has a rough jagged edge with bark still on. The project is to be a coffee table. The rectangular size for the whole table will be 88x64x5cm so it is fairly large. I have calculated the amount of resin needed and will be roughly 5kg worth of it. I will make a plywood box for the mould lined with mould release. Is clear polyester resin suitable for this table and if so would I be able to do the resin in one go.
Many thanks
Tags
Polyester
Resin
table
Reply
Like
13
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Is clear polyester resin suitable for encapsulating a rough bit of yew wood with bark on?
jruck
-
11 Years Ago
Our Waterclear Polyester CastingResin would work for this project with a couple of...
Warren (Staff)
-
11 Years Ago
Many thanks, However if I pour the resin in multiple layers would the layers be visible because i am...
jruck
-
11 Years Ago
You would see a very slight transition from the side. Reducing the catalyst ratio would help a...
Warren (Staff)
-
11 Years Ago
Warren great idea to dip the wood in the resin first, never thought of that before. But how about...
matthieutje65
-
11 Years Ago
You dip it just before you do the casting to get rid of the surface air entrapment. Lots of...
Warren (Staff)
-
11 Years Ago
I have used Polyester infusion resin for "impregnating/stabilizing wood.. I've found that I need to...
Dravis
-
11 Years Ago
Thanks for the info warren! Did some more research yesterday and found this video I thought is...
matthieutje65
-
11 Years Ago
A lot of the "stabilizing" of woods are done using Acrylic resins, they can have almost as low...
Dravis
-
11 Years Ago
Post Reply
Like
13
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search