Hi
Yesterday i really hammered the carbon lip on my front bumper, and it is really annoying.
Now i want to repair this myself, but i hope someone here can help me in the right direction.

If you look at the pictures you can see how the damage is.

Now my plan is to sand the whole lip down with 120grain wet sandpaper untill it seems even.
Then ill use a brush and apply epoxy laminating resin with a brush over the sanded area.
After this ill let the resin harden and then and it down with 800 and 1200 wet sandpaper.

Will this work and can i expect the reults to be pretty good?
Should i use anything to clean of the lip before applying the resin?

Any help appreciated
Attachments
carb.jpg (659 views, 71.00 KB)
carb2.jpg (608 views, 99.00 KB)
Replies
Ronny
Ronny
Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)
Group: Forum Members
Posts: 58, Visits: 401
I just did some research and it is a clear coating i need, for uv protection?
So ill add this to my list aswell, will be appyling the resin tomorrow, fingers crossed.
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
Yup, its for UV protection and also allows you to control the finish a bit more, gloss/satin etc... 

For your project, rattle can lacquer from Halfords or similar car part store would suffice 