Hi
Yesterday i really hammered the carbon lip on my front bumper, and it is really annoying.
Now i want to repair this myself, but i hope someone here can help me in the right direction.

If you look at the pictures you can see how the damage is.

Now my plan is to sand the whole lip down with 120grain wet sandpaper untill it seems even.
Then ill use a brush and apply epoxy laminating resin with a brush over the sanded area.
After this ill let the resin harden and then and it down with 800 and 1200 wet sandpaper.

Will this work and can i expect the reults to be pretty good?
Should i use anything to clean of the lip before applying the resin?

Any help appreciated
Attachments
carb.jpg (659 views, 71.00 KB)
carb2.jpg (608 views, 99.00 KB)
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
depending on how much you have tosand back you might get away with floodcoating of a 2k lacquer, rather than using resin as you will have to sand that back then polish to get a nice finsih
Ronny
Ronny
Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)
Group: Forum Members
Posts: 58, Visits: 401
At some parts i see right through to the carbon fibre, so all the resin is worn off.
This means i have to use resin right?
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
Sand, fill any deep bits with epoxy then lacquer.

It's non structural so don't worry about it too much, the white scars will go once you've sanded and lacquered 
Ronny
Ronny
Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)
Group: Forum Members
Posts: 58, Visits: 401

When you say lacquer, what product do you mean?
Could you point me to one type of lacquer product?

In my head the epoxy resin would both fill and once properly sanded and buffet it would get a nice clear surface.
Edited 10 Years Ago by Ronny
Ronny
Ronny
Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)
Group: Forum Members
Posts: 58, Visits: 401
I just did some research and it is a clear coating i need, for uv protection?
So ill add this to my list aswell, will be appyling the resin tomorrow, fingers crossed.
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
Yup, its for UV protection and also allows you to control the finish a bit more, gloss/satin etc... 

For your project, rattle can lacquer from Halfords or similar car part store would suffice 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search