Started an oven build today so thought i would make a thread to post my progress.
This is all new to me so I'm sure il have some questions on the way, and you can all correct me if i do something wrong BigGrin

Made the frame out of 15mm steel box tube



Then a 1mm steel outer skin



What size element would be good for this size oven?
Its 1 meter x 600mm x 600mm
Replies
taikuri
taikuri
Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)
Group: Forum Members
Posts: 13, Visits: 167
Thanks to this thread i build my oven, well its almost done and its almost similar. Made it 110cm x 100cm x 60cm and 2.5kw element, heats up pretty fast. Hardest part to find some rockwool with Alu foil on a top here in Spain.
Hopefully its ready in next few days. 
Darren
Darren
Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)
Group: Forum Members
Posts: 54, Visits: 916
taikuri (22/10/2015)
Thanks to this thread i build my oven, well its almost done and its almost similar. Made it 110cm x 100cm x 60cm and 2.5kw element, heats up pretty fast. Hardest part to find some rockwool with Alu foil on a top here in Spain.
Hopefully its ready in next few days. 




Im glad it helped you..

Mine works really well and holds the heat a lot better than i thought it would.

The hardest part was working out how to use the pid controller Hehe
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Darren - 11 Years Ago
Brian_s - 11 Years Ago
ChrisR - 11 Years Ago
Darren - 11 Years Ago
davro - 11 Years Ago
Darren - 11 Years Ago
     Vac innovations
f1rob - 11 Years Ago
ChrisR - 11 Years Ago
Shaneer22 - 11 Years Ago
wojtepanik - 11 Years Ago
AlessandroPA - 11 Years Ago
Darren - 11 Years Ago
AlessandroPA - 11 Years Ago
Darren - 11 Years Ago
Tones67 - 11 Years Ago
Jacopo Carbonio - 11 Years Ago
Hanaldo - 11 Years Ago
ChrisR - 11 Years Ago
Jacopo Carbonio - 11 Years Ago
taikuri - 11 Years Ago
Darren - 11 Years Ago
Jacopo Carbonio - 11 Years Ago
deceased10 - 10 Years Ago
67redrocket - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search