Started an oven build today so thought i would make a thread to post my progress.
This is all new to me so I'm sure il have some questions on the way, and you can all correct me if i do something wrong BigGrin

Made the frame out of 15mm steel box tube



Then a 1mm steel outer skin



What size element would be good for this size oven?
Its 1 meter x 600mm x 600mm
Brian_s
Brian_s
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
I hope you are going to insulate it? If so 2Kw will be ample.

Brian.
ChrisR
ChrisR
Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
and earth it!

Insulate the inside with celotex or similar, use a 2kW oven heater element and a fan with temperature process controller and you'll be well away
Darren
Darren
Supreme Being (658 reputation)Supreme Being (658 reputation)Supreme Being (658 reputation)Supreme Being (658 reputation)Supreme Being (658 reputation)Supreme Being (658 reputation)Supreme Being (658 reputation)Supreme Being (658 reputation)Supreme Being (658 reputation)
Group: Forum Members
Posts: 54, Visits: 916
Yeah I'm going to insulate it with 50mm celotex.

Where is the ideal place to mount the element? On the bottom or one of the sides?

Im thinking of getting a round element and having a fan in the middle of it (how most domestic ovens are)
davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Looking good so far! are you going to have any runners for shelves inside the oven.

I am about to start building my oven in the next week or so Wink



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Edited 11 Years Ago by davro
Darren
Darren
Supreme Being (658 reputation)Supreme Being (658 reputation)Supreme Being (658 reputation)Supreme Being (658 reputation)Supreme Being (658 reputation)Supreme Being (658 reputation)Supreme Being (658 reputation)Supreme Being (658 reputation)Supreme Being (658 reputation)
Group: Forum Members
Posts: 54, Visits: 916
davro (01/05/2015)
Looking good so far! are you going to have any runners for shelves inside the oven.

I am about to start building my oven in the next week or so Wink




I'm just going to have one fixed shelf in it.





Any body know a good place to buy vac fittings?
f1rob
f1rob
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Vac innovations
ChrisR
ChrisR
Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
I would also recommend VacInnovations, they have all the kit you could possibly need and whenever I have rung them they have been helpful.
Shaneer22
Shaneer22
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
Any more progress.
wojtepanik
wojtepanik
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 102, Visits: 582
looks badass !! keep us informing ! Smile

~~~Everytime I hear sound of demoulding part I have eargasm~~~
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search