Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Some opinions on this thread
Some opinions on this thread
Post Reply
Like
2
Some opinions on this thread
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
baja_patient
baja_patient
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 135,
Visits: 1.6K
Hi guys, was browsing the net looking for some information on this and that. Came across the composites central forum and read a post regarding the EC video on perfect resin infusion and the ensuing discussion.
http://www.compositescentral.com/showthread.php?t=5092
They question some of the methods in the video, some say to leave the pump running til gelation/cure, others dont.
Care to take a read of the short thread and give some feedback?
It has definitely caused me some confusion.
Cheers
Reply
Like
2
Reply
Warren
Warren
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 214,
Visits: 782
I spoke with Matt this afternoon about spray tack, they are just waiting on it being shipped over.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Some opinions on this thread
baja_patient
-
13 Years Ago
Hi Fabian, Some people on the Composites Central thread may be missunderstanding what that video...
Matt (Staff)
-
13 Years Ago
Hi Matt I totally agree with you. The single most important thing I have learned from you is the...
fgayford
-
13 Years Ago
Hi Matt, Yes absolutely!clears it up for me thanks alot. I have no doubt you guys have the...
baja_patient
-
13 Years Ago
I spoke with Matt this afternoon about spray tack, they are just waiting on it being shipped over.
Warren
-
13 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search