Hi guys, was browsing the net looking for some information on this and that. Came across the composites central forum and read a post regarding the EC video on perfect resin infusion and the ensuing discussion.
http://www.compositescentral.com/showthread.php?t=5092
They question some of the methods in the video, some say to leave the pump running til gelation/cure, others dont.
Care to take a read of the short thread and give some feedback?
It has definitely caused me some confusion.
Cheers
By fgayford
-
11/10/2012 2:12:35 AM
Hi Matt
I totally agree with you.
The single most important thing I have learned from you is the turning off of the vacuum pump. Thats a scarey deal if you don't have your confidence up.Who would ever think of closing off the lines in the first place! It wouldn't have occurred to me. The first time I did and got no pinholes I became a believer. (of course the resin viscosity was the other part of the puzzle I had to overcome. Heating the mold and the resin first).
Yes for compaction and strength you want the pump running, but for cosmetic parts it is a totally different story.
Thanks Again!