So thinking of getting some proper heating in the garage and wondering what you guys recommend.

I unable to spend loads on professional fitted kit so was thinking butane heater, paraffin heater, halogen etc.

most interested to know if I can use infra red lights, could I use these to cure as well as give general room heat.

Chris.
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Very good solution is to use electric blankets. No good for post-cure temperatures, but great for initial cure temps. 