garage heating / resin curing


Author
Message
Brian2fast
Brian2fast
Supreme Being (631 reputation)Supreme Being (631 reputation)Supreme Being (631 reputation)Supreme Being (631 reputation)Supreme Being (631 reputation)Supreme Being (631 reputation)Supreme Being (631 reputation)Supreme Being (631 reputation)Supreme Being (631 reputation)
Group: Forum Members
Posts: 79, Visits: 1.3K
I insulated the roof of my single garage/workshop a few years ago and now I can keep a constant 20 degree C with a 4kw fan heater. I also use an additional  2 kW heater and iv had the area on my bench upto 40 deg C.
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
If your mould/part is small enough then you can also make a temp tent over it with a foot heater blowing in under it, just put a few weights around the edge and a let some of the air blow out the other end.

I use the very light disposable painters drop sheets from the hardware shop as they are so light they just float up into a nice balloon type tent.




I also recently used an LPG flame type heater/blower to heat my workshop for a particular infusion job, it worked fine but the fumes from burning LPG fill the shop and are really unpleasant.







Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Very good solution is to use electric blankets. No good for post-cure temperatures, but great for initial cure temps. 
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
ok so stay away from open flame heaters.

like the look of the infra red ones but on reading the paint guys use short wave lights as opposed to long wave (cheaper) ones.
Zorongo
Zorongo
Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)
Group: Forum Members
Posts: 40, Visits: 330
Beware "open flame" (direct) heaters by two reasons: By one side may be an explosion owed to aceton or other vapours. The other side, the open flame produces rests that con end over your molds's surfaces and inhibit resin´s curing.
jaffa
jaffa
Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)
Group: Forum Members
Posts: 17, Visits: 325
I bought a 3kw fan heater and tried to draught proof the garage as much as possible for when I'm infusing. Be interested to hear other opinions as i'm a beginner

Happy with the results I've had though
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
So thinking of getting some proper heating in the garage and wondering what you guys recommend.

I unable to spend loads on professional fitted kit so was thinking butane heater, paraffin heater, halogen etc.

most interested to know if I can use infra red lights, could I use these to cure as well as give general room heat.

Chris.