Hi all.

I'm making small size epoxy parts, but sometimes I've made them whith polyester. Room temperature curing, hand lay up with small presure over the laminate (counter mold)

I had demolding problems with a polyester mold and someone told me a "rule of thumb": Use polyester molds for polyester parts and epoxy molds for epoxy parts.

(I'm actualy using PE molds for epoxy parts without any problem) So, the question is: Whe should I use epoxy molds ?

An epoxy mold seems to be better fron the dimensional stability point of view..

It also seems logical to make the molld similar to the part if high temp increases are expected (prepregs, exotherms ?) to reach a similar diatation / contraction on both and avoiding stresses....

Could you please share your experience ?

Thanks in advance Wink
Reply
Zorongo
Zorongo
Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)
Group: Forum Members
Posts: 40, Visits: 330
Thanks for the answers.

I didn't pay attention to the styrene matter.

I've been using PE molds for Epoxy parts and normally without any problem. So I thought it was more a question of the release agent as following same process one wax gave me best results than other.

I was thinking on PVA a a phisycal barrier, too....




Probabily I'll go to VE for next ones. And maybe postcuring to evaporate styrene. (And maybe also a layer of PVA "jaust in case"?)

Thanks again ! Wink
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search