not to thread jack but I have a question along these lines. My uncle has some motorcycle fender molds he no longer uses and they will work good with my bike. The molds are over 10 years old but still in good shape as they were made thick and with braces to stop as much warping as possible. I am wanting to use epoxy resin to make some carbon fiber fenders, but the molds were made with PE resin. If I use PVA on the molds and since they are old. WIll this be a problem? I am only producing these for myself and would like to avoid mold making costs if at all possible. I am wanting to infuse the fenders. If it will be, then I will make new molds. These are universal chopper fenders and there could be a call for more if I marketed them to help with mold costs, but im terrible with that stuff lol
|