Group: Forum Members
Posts: 43,
Visits: 109
|
I usually use pva without wax on my polyester mould.. Before laying cf I brush a layer of epoxy gelcoat transparent (this is the reason why I don't use wax).. Sometimes I have problems with demoulding because of the shape (it sticks a little).. With chemical release or similar will be better?
|