Can i use Infusion resin for laminating?


Author
Message
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Small simple question...

till now I have mostly done Infusions on carbon parts but now I have a small part I would like to laminate...

I have some IN2 epoxy resin (for infusion)

would it cause any problems if I laminate with this?

it would be a simple part with Carbon and Kevlar sheets with dimension of 30cmx30cm... I planned to laminate the sheets on plastic foils and then allign them into the mould...

than vacuumbag it...

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com