By matthieutje65 - 4/24/2012 11:28:48 PM				
            
                      
            Small simple question... 
  till now I have mostly done Infusions on carbon parts but now I have a small part I would like to laminate...
  I have some IN2 epoxy resin (for infusion)
  would it cause any problems if I laminate with this? 
  it would be a simple part with Carbon and Kevlar sheets with dimension of 30cmx30cm... I planned to laminate the sheets on plastic foils and then allign them into the mould...
  than vacuumbag it...
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Joe - 4/25/2012 5:22:18 PM				
            
                      
            Hi, 
  To complete what Paul said about using laminating resins in infusion, 
  http://www.talkcomposites.com/299/Infusion-With-High-Temp-resin
           
		 | 			
		 
	
	
						
		 	
		
	 |