Hi Matthieu,
The simple Answer for your simple question is yes! The infusion resin is simply a lower viscosity version of the laminating resin, for flatter components it's great however for vertical face (like up the side of a mould) the resin can drain away which is the primary reason for the laminating resin being higher viscosity. likewise the laminating resin can be used for infusion, however it will infuse much slower so this is only a possibility for very small parts.
Paul Statham Easy Composites / Carbon Mods - Technical
|