I have been working with carbon fiber since this year so I'm still a rookie I would say. I doing some CF myself and I'm wondering if I could use pre preg to do laminations of the nterior trim ?
Reply
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Best idea if you're just wanting the cosmetics is to wrap the part wet lay style