Car instrument binnacle has turned Yellow
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Alibro
Alibro
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 44,
Visits: 384
Hi Guys
I wrapped the instrument binnacle on my little MGF and was very happy with how it looked. Not perfect by any means but everyone who saw it was impressed. Recently however the car has been kept outside more than before and it has started to go Yellow. I used Gurit SP106 and lacquered with Halfords lacquer which is supposed to be UV resistant.
http://www.halfords.com/motoring/paints-body-repairs/car-spray-paints/halfords-clear-lacquer-500ml
Is this normal?
Did I use the wrong epoxy?
Did I use the wrong Lacquer?
Since wrapping this part I have got a compressor and spray gun so can use a better lacquer for new parts but not sure what to ask for at the paint shop.
Any advice gratefully accepted.
This is what I did.
Reply
Like
2
Reply
FLD
FLD
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 2.7K
Cheap lacquer turns yellow I'm afraid.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Car instrument binnacle has turned Yellow
Alibro
-
11 Years Ago
Once the part has cured but before you install it, sand it with 600grit wet sand paper to smooth it...
kidpaint
-
11 Years Ago
Cheap lacquer turns yellow I'm afraid.
FLD
-
11 Years Ago
Thanks guys, I will try to find a proper paint supplier in my area. Now I have a compressor I can...
Alibro
-
11 Years Ago
Be careful when spraying the clear on your parts. It can be very hazardous to your health. Where...
kidpaint
-
11 Years Ago
Good advice Kidpaint, I have heard a lot of bad things about 2k paint so will try to avoid it if I...
Alibro
-
11 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search