I have laminated a carbon frame tube using 3k 2x2 and unidirectional carbon, Using vacuum bagging! wrinkles have appeared after demould and i wondered why , is the bagging too loose , any advice or tips greatly appreciated!
Replies
whereismillar
whereismillar
Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)
Group: Forum Members
Posts: 10, Visits: 31
Hi mathieu

No the carbon itself is wrinkled after removing everything post cure! where the vacuum bag itself was wrinkled when using the pump and curing
no pictures yet but will post some tomorrow
before bagging the carbon , peel ply , perforated film, and breather cloth were carefully applied!

.
Edited 11 Years Ago by whereismillar
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Ok, I'll wait for some images Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
whereismillar - 11 Years Ago
matthieutje65 - 11 Years Ago
whereismillar - 11 Years Ago
             Ok, I'll wait for some images :)
matthieutje65 - 11 Years Ago
ChrisR - 11 Years Ago
whereismillar - 11 Years Ago
ajb100 - 11 Years Ago
whereismillar - 11 Years Ago
matthieutje65 - 11 Years Ago
ChrisR - 11 Years Ago
whereismillar - 11 Years Ago
ChrisR - 11 Years Ago
Zorongo - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search