I have laminated a carbon frame tube using 3k 2x2 and unidirectional carbon, Using vacuum bagging! wrinkles have appeared after demould and i wondered why , is the bagging too loose , any advice or tips greatly appreciated!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
whereismillar - 11 Years Ago
matthieutje65 - 11 Years Ago
whereismillar - 11 Years Ago
             Ok, I'll wait for some images :)
matthieutje65 - 11 Years Ago
ChrisR - 11 Years Ago
whereismillar - 11 Years Ago
ajb100 - 11 Years Ago
whereismillar - 11 Years Ago
matthieutje65 - 11 Years Ago
ChrisR - 11 Years Ago
whereismillar - 11 Years Ago
ChrisR - 11 Years Ago
Zorongo - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search