	Group: Forum Members 	        
    Posts: 99, 
    Visits: 2.5K 
    
 
          
		     | 
				                       
                 
                
                    
			            Yes it is made to be played. It sounds great. My wife has a wooden one that this is based on. As the weather changes, the wood moves and it goes out of tune. I thought Carbon Fibre would be more stable. I am just waiting for the strings to settle down. (Nylon strings stretch and go out of tune for a few days.) Then I will record my wife playing it.
  Cost, including making the moulds and vacuum equipment (I already had a vacuum pump.) are about £700 plus £70 for harp tuning pins and strings etc.
  I have learned a lot from making this.
  Brian.                
			            				
			                                 
                     
                                            
                         
                    
                  
             |