If your budget allows get yourself a Dremel and some slitting disks. If not a jigsaw with a metal cutting blade or a hacksaw will all work well. Just put some masking tape along the cut line. Standard metal working files, a sanding block and wet and dry will finish edges nicely. If drilling holes etc use masking tape again and support the back of the part on a block of wood if possible to reduce break out, or if you can clamp the part between two pieces of wood and drill through the whole stack.
Warren
Carbon Copies Ltd
|