Could anyone recommend Finishing tools, files etc for CF - that are available in the UK?
I know about Perma-Grit, but don't have Perma-Grit cash flow
.
Thanks,
Adam
By FLD
-
9/24/2013 3:46:47 PM
I find anything diamond coated to be good. For example, I picked up a set of diamond coated files from TK Maxx for 6 quid and they're great! The only downside with regular metalworking tools is that they blunt off quite quickly with composites. I knackered a few bandsaw blades this way before buying diamond coated cutting discs (silverline ones from ebay, cut quicker than the permagrit one I have!!).