Has anybody tried laying up several flat sheets at once, each separated by a caul sheet?

Each sheet Im doing is 600g Diolen, 600g glass, 1000mmx1200mm.

I need to do a run, so thought of laying 5 sheets, stacking them with aluminium sheets as separators.
If anyone has tried this, can they please reply with any issues I might encounter

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
Edited 12 Years Ago by carboncactus
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search