Talk Composites - The Forum for Advanced Composites

Several flat sheets at once

http://www.talkcomposites.com/Topic6803.aspx

By carboncactus - 6/26/2013 1:45:37 PM

Has anybody tried laying up several flat sheets at once, each separated by a caul sheet?

Each sheet Im doing is 600g Diolen, 600g glass, 1000mmx1200mm.

I need to do a run, so thought of laying 5 sheets, stacking them with aluminium sheets as separators.
If anyone has tried this, can they please reply with any issues I might encounter
By wozza - 6/26/2013 2:24:14 PM

Ooooooops sorry Ermm The only real issue I can see is evacuating the air from between the ply's. But that is just me thinking out load Smile