Heavy dutty flexible carbon fiber


Author
Message
kylle
kylle
Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)
Group: Forum Members
Posts: 34, Visits: 101
Matt (Staff) (22/02/2012)
Hi Kylle,

The thick flexible sheet can't really be re-formed using heat. It would respond to some extend but I don't think it's going to give you the results you're after. I did mention in another thread our new flexible epoxy resin. I think this might be a good idea for what you're working on here. Perhaps this is what you had in mind when you asked about the flexible epoxy?

--Matt


Yes it was matt! 
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Kylle,

The thick flexible sheet can't really be re-formed using heat. It would respond to some extend but I don't think it's going to give you the results you're after. I did mention in another thread our new flexible epoxy resin. I think this might be a good idea for what you're working on here. Perhaps this is what you had in mind when you asked about the flexible epoxy?

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
kylle
kylle
Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)
Group: Forum Members
Posts: 34, Visits: 101
Already seen the sample Paul(thanks E.C.)! I think it will work but the angles are to tight to glue in the bike frame.
Can it be moulded  applying heat ?
Currently its in place using zip ties but the chain strikes the zip-ties and breaks them! If the sheet hold position I could glue it to the frame without the hazard of the protection hitting the back wheel or the spokes.
It almost look like this:

Paul (Staff)
Paul (Staff)
Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)
Group: Administrators
Posts: 134, Visits: 614
Hi Kyle,

It would certainly take the abuse, it is a 2.5 thick material commonly used for mudflaps, but it may not curve very easily to your chainstay, if it's a box-section chainstay you could just apply it to the top face and I'm sure it would be fine.

The other thing to note is that it doesn't have a self adhesive backing, I'm sure a high quality double-sided tape will work to do the job.

I'll get the image on the product page very shortly.

Paul Statham
Easy Composites / Carbon Mods - Technical
kylle
kylle
Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)
Group: Forum Members
Posts: 34, Visits: 101
Can you provide a picture of the heavy dutty carbon fiber? I'm using a normal flexible carbon fiver bought in easy composites in a chainstay of my bike but the clear transparent layer it's starting to peel off and It haves few hours of practice.... It's a downhill bike... the rear section takes a lot of bumps and the chain hits the frame A LOT....
Will the heavy dutty flexible CF work?