Heavy dutty flexible carbon fiber


Author
Message
kylle
kylle
Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)
Group: Forum Members
Posts: 34, Visits: 101
Can you provide a picture of the heavy dutty carbon fiber? I'm using a normal flexible carbon fiver bought in easy composites in a chainstay of my bike but the clear transparent layer it's starting to peel off and It haves few hours of practice.... It's a downhill bike... the rear section takes a lot of bumps and the chain hits the frame A LOT....
Will the heavy dutty flexible CF work?