gel coat color


Author
Message
ana
a
ana
posted 5 Years Ago HOT
Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)
Group: Forum Members
Posts: 14, Visits: 49
Dear friends
hi
i am applying gel coat on fiberglass mold . for dark color i need to reach matte color
""
 apaqua " surface .

i add some fillers but i did not reach perfect color .

please help me what can i add to normal pigment paste to reach matte surface ?
i do not want shinny surface .

tanks in advance
regards
ana