Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Hand Layup
»
gel coat color
gel coat color
Post Reply
Like
4
gel coat color
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
ana
a
ana
posted 4 Years Ago
ANSWER
HOT
Topic Details
a
Group: Forum Members
Posts: 14,
Visits: 49
Dear friends
hi
i am applying gel coat on fiberglass mold . for dark color i need to reach matte color
""
apaqua " surface
.
i add some fillers but i did not reach perfect color .
please help me what can i add to normal pigment paste to reach matte surface ?
i do not want shinny surface .
tanks in advance
regards
ana
Edited
4 Years Ago by
ana
Reply
Like
4
Reply
Hanaldo
Hanaldo
posted 4 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
You can't get a matte finish out of a shiny mould. Only way to sort of do it is to spray PVA release agent as a 'dust' to take the shine away. But it isn't a true matte, its more of a texture.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
gel coat color
ana
-
4 Years Ago
You can't get a matte finish out of a shiny mould. Only way to sort of do it is to spray PVA release agent as a 'dust' to take the shine away. But it isn't a true matte, its more of a texture.
Hanaldo
-
4 Years Ago
You can get a good matt finish post demoulding with a satin/matt lacquer. However as Hanaldo said, no way to really get it a matt finish straight from the mould.
Warren (Staff)
-
4 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search