By ana - 3/14/2021 6:52:11 AM
Dear friends hi i am applying gel coat on fiberglass mold . for dark color i need to reach matte color "" apaqua " surface . i add some fillers but i did not reach perfect color .
please help me what can i add to normal pigment paste to reach matte surface ? i do not want shinny surface .
tanks in advance regards ana
|
By Warren (Staff) - 3/15/2021 9:40:06 AM
You can get a good matt finish post demoulding with a satin/matt lacquer. However as Hanaldo said, no way to really get it a matt finish straight from the mould.
|
|