gel coat color


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You can get a good matt finish post demoulding with a satin/matt lacquer.  However as Hanaldo said, no way to really get it a matt finish straight from the mould. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Hanaldo
Hanaldo
Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You can't get a matte finish out of a shiny mould. Only way to sort of do it is to spray PVA release agent as a 'dust' to take the shine away. But it isn't a true matte, its more of a texture. 
ana
a
ana
posted 5 Years Ago HOT
Supreme Being (250 reputation)Supreme Being (250 reputation)Supreme Being (250 reputation)Supreme Being (250 reputation)Supreme Being (250 reputation)Supreme Being (250 reputation)Supreme Being (250 reputation)Supreme Being (250 reputation)Supreme Being (250 reputation)
Group: Forum Members
Posts: 14, Visits: 49
Dear friends
hi
i am applying gel coat on fiberglass mold . for dark color i need to reach matte color
""
 apaqua " surface .

i add some fillers but i did not reach perfect color .

please help me what can i add to normal pigment paste to reach matte surface ?
i do not want shinny surface .

tanks in advance
regards
ana
Edited 5 Years Ago by ana