I need to make some 90 degree angles. I also need them to be gloss on both sides. I tried make to separate angles and then glue them with 2 part epoxy glue but they are not as stiff as i need them to be and there is some delamination when i apply pressure on them. What can i do so i can have a gloss finish on both sides? 
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Try two nice and thick aluminium angle sections then wet lay and do a bit of compression moulding by clamping them together.  You can put them in a vacuum bag with a bit of breather to do the same thing.  Just make sure everything is nicely release coated for when the excess resin squeezes out. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Elias_GR
Elias_GR
Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)
Group: Forum Members
Posts: 11, Visits: 604
Thanks a lot for the answer Warren! 
This is exactly the first idea i had for them.
I did them exactly like how you described it but i got a lot of dry spots in the fabrics and a lot pinholes. Maybe i applied too much or too little pressure? I can't tell for sure but I tried it more than 6 times and i only got once or twice a good looking result. 
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
For most wet lay vacuum bagging you want about 20% vacuum to start with then adjust to suit the results. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search