Hi, I have a part which is "d" shaped with flanges on the edges and surface about 1.5 m2.
I am willing to use Lantor Soric XF as a core for my infusion and I know that infusion mesh could be avoided.
I will be more comfortable with the standard process (peelply, infusion mesh, bag).
Will it hurt in any way if I will infuse with the standard stack?