Group: Forum Members
Posts: 167,
Visits: 1.1K
|
Hi, I have a part which is "d" shaped with flanges on the edges and surface about 1.5 m2. I am willing to use Lantor Soric XF as a core for my infusion and I know that infusion mesh could be avoided. I will be more comfortable with the standard process (peelply, infusion mesh, bag). Will it hurt in any way if I will infuse with the standard stack?
|