Hi, I have a part which is "d" shaped with flanges on the edges and surface about 1.5 m2.
I am willing to use Lantor Soric XF as a core for my infusion and I know that infusion mesh could be avoided.
I will be more comfortable with the standard process (peelply, infusion mesh, bag).
Will it hurt in any way if I will infuse with the standard stack?
Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
No not at all, in fact really it is better - Soric and other internal flow medias flow quite slowly in comparison to regular flow mesh, and depending on your layup they can make pinholes more likely.

The downside is that you use a lot more resin.
Massimiliano
M
Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hanaldo - 11/13/2020 9:25:42 AM
No not at all, in fact really it is better - Soric and other internal flow medias flow quite slowly in comparison to regular flow mesh, and depending on your layup they can make pinholes more likely.

The downside is that you use a lot more resin.

Thank you Hanaldo. 
I'd rather prefer to use more resin than to have gel before the infusion is over 😅