Hi

I need to skin a motorcycle fender with cf, but it is in raw metal.

Do i have to aplly some primer first, to prevent the appearence of rust?

Pedro
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
pedcrist - 14 Years Ago
Matt (Staff) - 14 Years Ago
marc37i - 14 Years Ago
Matt (Staff) - 14 Years Ago
marc37i - 14 Years Ago
     etch the metal
Jack.Strong - 14 Years Ago
Kevin-Lee - 14 Years Ago
pedcrist - 14 Years Ago
Matt (Staff) - 14 Years Ago
marc37i - 14 Years Ago
Matt (Staff) - 14 Years Ago
marc37i - 14 Years Ago
Matt (Staff) - 14 Years Ago
     Thanks Matt
marc37i - 14 Years Ago
mhdghoul - 14 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search