Epoxy bonds to epoxy when the epoxy you're bonding to is in the 'B' stage of its cure; this allows the fresh epoxy to cross link to the 'B' stage cured epoxy and make a strong chemical bond. Once the first layer of epoxy has fully cured, the cross linking won't happen and the new epoxy will only be able to make a mechanical bond to the first layer of epoxy which is less strong so, although it bonds well (given the appropriate surface preparation/key) it won't be as strong as a bond to 'tacky' (b stage) epoxy.