By pedcrist - 12/3/2012 1:59:01 PM
Hi
I need to skin a motorcycle fender with cf, but it is in raw metal.
Do i have to aplly some primer first, to prevent the appearence of rust?
Pedro
|
By mhdghoul - 12/21/2012 5:44:19 PM
number 1 is gr8 as an option ,u dont have to go through the headeack of removing it, conside it as a great primer ,u may use the black base coat i think it will show nothing like metal below , hope this is fruitfull