pedcrist
pedcrist
Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)
Group: Forum Members
Posts: 42, Visits: 350
Hi

I need to skin a motorcycle fender with cf, but it is in raw metal.

Do i have to aplly some primer first, to prevent the appearence of rust?

Pedro
Reply
marc37i
marc37i
Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)
Group: Forum Members
Posts: 16, Visits: 566
Matt (Staff) (04/12/2012)
Hi Marc,

The bond would be better to bare, keyed, metal than it would to the plastic of the paint. Likewise, I would say that the bond of the epoxy to the metal would also be better than the bond of the paint to the metal too so if you have a choice then bare metal is the way to go.

--Matt



Thanks Matt :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
pedcrist - 13 Years Ago
Matt (Staff) - 13 Years Ago
marc37i - 13 Years Ago
Matt (Staff) - 13 Years Ago
marc37i - 13 Years Ago
     etch the metal
Jack.Strong - 13 Years Ago
Kevin-Lee - 13 Years Ago
pedcrist - 13 Years Ago
Matt (Staff) - 13 Years Ago
marc37i - 13 Years Ago
Matt (Staff) - 13 Years Ago
marc37i - 13 Years Ago
Matt (Staff) - 13 Years Ago
     Thanks Matt
marc37i - 13 Years Ago
mhdghoul - 13 Years Ago