Hello,
I tried making tubes by wrapping prepreg around POM rod without using any release agent. after removing the part from oven, due to the thermal expansion of the POM rod, the cured tube jut slipped out.
I was curious to know if anyone has made tubes using other types of plastics( PTFE Teflon, PET, ) as a mandrel.
would be great to share your experiences