using plastic tubes as a mandrel


Author
Message
Lester Populaire
L
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
POM is one of the best materials in my opinion. PTFE would probably work even better due to the higher temperature stability, but isn't necessary and expensive. And to avoid deformation i would recommend to rest the tube in an aluminum angle extrusion during curing so everything stays straight.
Fasta
Fasta
Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
hadi1990 - 5/3/2020 1:51:13 PM
Hello,
I tried making tubes by wrapping prepreg around POM rod without using any release agent. after removing the part from oven, due to the thermal expansion of the POM rod, the cured tube jut slipped out.
I was curious to know if anyone has made tubes using other types of plastics( PTFE Teflon, PET, ) as a mandrel.
would be great to share your experiences

I have done a few s mall parts with Delrin as a mandrel/core and it work great. Yes there is a reasonable amount of expansion and the parts just fall out without the need for any release agents.

Not sure how it would go with a length as it may bend ??






hadi1990
h
Supreme Being (277 reputation)Supreme Being (277 reputation)Supreme Being (277 reputation)Supreme Being (277 reputation)Supreme Being (277 reputation)Supreme Being (277 reputation)Supreme Being (277 reputation)Supreme Being (277 reputation)Supreme Being (277 reputation)
Group: Forum Members
Posts: 15, Visits: 651
Hello,
I tried making tubes by wrapping prepreg around POM rod without using any release agent. after removing the part from oven, due to the thermal expansion of the POM rod, the cured tube jut slipped out.
I was curious to know if anyone has made tubes using other types of plastics( PTFE Teflon, PET, ) as a mandrel.
would be great to share your experiences