Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
ยป
Advanced Composites Forum
ยป
Pattern and Plug Making
ยป
Cut through Hi Gloss
Cut through Hi Gloss
Post Reply
Like
4
Cut through Hi Gloss
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Massimiliano
M
Massimiliano
posted 6 Years Ago
ANSWER
HOT
Topic Details
M
Group: Forum Members
Posts: 167,
Visits: 1.1K
Hi, after countless hours sanding the Pattern Coat Hi Gloss, I ended up removing too much and now I have a small area (about 3 cm) with Pattern Coat Primer exposed.
Please see picture.
Is there any way I can go on up with the next grits (600, 800, 1000, 1500, polish) and cover the area (filleting wax? Mold release wax? Magic?) so I can get a shining area like the surrounding one?
Please please don't tell me I have to cover back with Hi Gloss and start sanding again ... it has been so hard and long to remove the low spots left by the brush.
Thanks
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Cut through Hi Gloss
mporta71
-
6 Years Ago
You wont get it up to the same shine on the pattern without recoating.The good news is you should be able to mould off the primer anyway, so I would just proceed with making the mould and then polish...
Hanaldo
-
6 Years Ago
Thanks a lot!
mporta71
-
6 Years Ago
I did as you suggested and worked perfectly! Thank you!
mporta71
-
6 Years Ago
Excellent ๐๐
Hanaldo
-
6 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search