By mporta71 - 4/25/2020 2:06:07 PM
Hi, after countless hours sanding the Pattern Coat Hi Gloss, I ended up removing too much and now I have a small area (about 3 cm) with Pattern Coat Primer exposed. Please see picture.
Is there any way I can go on up with the next grits (600, 800, 1000, 1500, polish) and cover the area (filleting wax? Mold release wax? Magic?) so I can get a shining area like the surrounding one?
Please please don't tell me I have to cover back with Hi Gloss and start sanding again ... it has been so hard and long to remove the low spots left by the brush. Thanks
|
By Hanaldo - 5/9/2020 8:38:22 AM
Excellent ๐๐
|
|