	Group: Forum MembersPosts: 2.5K, 
    Visits: 28K
 
 | 
                    
			            You wont get it up to the same shine on the pattern without recoating. The good news is you should be able to mould off the primer anyway, so I would just proceed with making the mould and then polish that area out of the mould.  
 When you do your release agent, I would do the 6-8 coats of Easylease and then do 2 coats of release wax on top of that. Should guarantee you don't have any issues with porosity in the exposed primer.
 
 |