+x Hanaldo - 4/25/2020 3:30:56 PMYou wont get it up to the same shine on the pattern without recoating. The good news is you should be able to mould off the primer anyway, so I would just proceed with making the mould and then polish that area out of the mould. When you do your release agent, I would do the 6-8 coats of Easylease and then do 2 coats of release wax on top of that. Should guarantee you don't have any issues with porosity in the exposed primer.
+x Massimiliano - 4/25/2020 3:35:05 PM+x Hanaldo - 4/25/2020 3:30:56 PMYou wont get it up to the same shine on the pattern without recoating. The good news is you should be able to mould off the primer anyway, so I would just proceed with making the mould and then polish that area out of the mould. When you do your release agent, I would do the 6-8 coats of Easylease and then do 2 coats of release wax on top of that. Should guarantee you don't have any issues with porosity in the exposed primer.Thanks a lot!