Hi guys
I have been cutting and trimming Carbon with the following.
Dremel Tool - Jigsaw with a carbid grit blade - 4 inch cut off wheel - Vibrator Tool - Chisel
I am about to make a Carbon Fiber Violin of a Strad 1701 copy that I just bought for that purpose.
If you have ever looked at the F holes you can see the problems of the fine cuts involved.
What would be the best way? A 3d water jet would probably be the best, but real expensive.
Have you guys had any experience where real fine perfect cuts are involved?
Or could a steady hand with a dremel also get me there. Perhaps used like a router with a template guide.
Which cutters are the best? Carbid Diamond .
Thanks